DPA-4.1-Air-OAM
Model overview
Interatomic potential: Energy with gradient-based forces and stress.
CPS 0.893 combines discovery, geometry optimization, and phonons. Inspect individual task results below.
Licenses are as declared by the submitter. Training dataset terms are listed separately below.
Click a task score to show this model's diagnostics below.
Model info
Specifications
- Architecture
- gnn
- Outputs
- Energy with gradient-based forces and stress EFSG
- Openness
- Open source, open data OSOD
Discovery protocol
- Training
- structure to energy, force, stress S2EFS
- Evaluation
- initial structure to relaxed energy with structure relaxation IS2RE-SR
Training set
MPtrj: 1.58M structures from 146k materials · MIT
OMat24: 101M structures from 3.23M materials · CC-BY-4.0
Subsampled Alexandria: 10.4M structures from 3.23M materials · CC-BY-4.0
Trained by
Description
DPA-4.1-Air-OAM is a 5.1-million-parameter DPA4 interatomic potential trained on MPtrj, OMat24 and sAlex. Its SE(3)-equivariant architecture combines angular-degree coupling in SO(2) convolutions, multi-focus representations, attention and Wigner bilinear nonlinearities. Forces and stresses are derived from a single energy model.
Evaluation
Per-structure relaxation convergence and iteration counts were not recorded. MD energy and force RMSEs are not reported because the labeled reference data are not publicly available. The submitted κ-103 predictions for CuH (mp-24093) did not come from the submitted FC2/FC3 forces (κ 5.11 vs 4.86 W/mK when refit from them). The maintainers recomputed that row's frequencies and κ from the stored forces with the original phono3py pipeline. The other 102 rows are unchanged, and the original file remains on Figshare.
Diatomics
Some homonuclear pairs, especially Ne, exhibit large errors and numerical sensitivity at short separations. No elements were excluded from the metrics.
Disclosure
The DPA4 paper (arXiv:2606.02419, Methods 4.1 and Supp. S-3) chose architecture and training-schedule defaults with ablations evaluated on a fixed subsample of the WBM test set, so WBM informed model development.
Hyperparams
Dependencies (3)
Run this model
Use the submitted environment with the upstream instructions.
From a repository checkout, run uv run models/run_kappa.py --list-models to check checkpoint requirements. If this model requires one, add --checkpoint /path/to/checkpoint below. Then execute the printed command
for a phonon smoke test in the model's isolated environment.
uv run models/run_kappa.py --model dpa-4.1-air-oam --print-cmd --dry-run